Abstract:
A new kind of zirconia matrix ceramic material (ZrO2/Al2O3) is developed with 3Y-PSZ(3% Y2O3 partially stabilized ZrO2) and the additive of alumina. The wear resistance of ZYA20 (3Y-PSZ+20%
Al2O3) is experimentally investigated comparing with ZYA30 (3Y-PSZ+30%
Al2O3) by the wear ring-block test. It is shown that the friction coefficients of ZYA20 and ZYA30 decrease with the increment of the applied load and the wear ratios increase with the increment of the applied load. It is also found that their wear mechanisms are plastic deformation, adhesive and abrasive wear as well as stripping. The wear resistance of ZYA20 and ZYA30 is very good at low load and the former is stronger than the latter.
Key words:
Composite ceramics Spinning and weaving scissors Wear resistance
* This project is supported by Provincial Natural Science Foundation of Shandong (No.Y2001F05) and Young Research Star Foundation of Jinan, China (No.20110).Selected
from Proceedings of International Symposium of Advanced Manufacturing
Technology (ISAMT'2001); revised manuscript July 15, 2002
|